What Are 1.4306 and 1.4307?

1.4306 (X2CrNi19-11) and 1.4307 (X2CrNi18-9) are two European designations within the low-carbon austenitic stainless steel family that the market knows as AISI 304L. Both share the same chromium level, the same very low carbon content and the same fully austenitic structure, which gives them excellent weldability, good formability and cleanliness that suits hygienic service.

The difference between them is nickel. 1.4306 carries a higher nickel addition, and that single change shifts corrosion performance, phase stability after welding and the purchase price. For engineers, procurement teams and fabricators the choice usually comes down to whether the extra nickel is genuinely needed by the service environment or whether the standard grade will do the job at lower cost.

Equivalent Grades and Chemical Composition

Standard 1.4306 1.4307
EN / ISO designation X2CrNi19-11 X2CrNi18-9
AISI / ASTM 304L, higher nickel variant 304L, standard
UNS S30403 S30403
JIS SUS 304L high nickel SUS 304L

Both grades fall under the same UNS number because S30403 controls the carbon content rather than the nickel level, which is why the JIS and EN designations are the practical way to distinguish them on a purchase order. The table below shows the specified ranges.

Element 1.4306 (X2CrNi19-11) 1.4307 (X2CrNi18-9)
Carbon 0.030% max 0.030% max
Chromium 18.0 - 20.0% 17.5 - 19.5%
Nickel 10.0 - 13.0% 8.0 - 10.5%
Manganese 2.00% max 2.00% max
Silicon 1.00% max 1.00% max
Sulphur 0.015% max 0.030% max

The EN designation of 1.4306 reflects an intended level of about 19% chromium and 11% nickel, while 1.4307 reflects about 18% chromium and 9% nickel. Note that the chromium range for 1.4306 is 18.0 - 20.0% under EN 10088, not the 17.5 - 19.5% range that applies to 1.4307, so the two grades are not interchangeable on analysis alone.

Mechanical and Physical Properties

Property 1.4306 1.4307
Yield strength Rp0.2 190 MPa min 190 MPa min
Tensile strength Rm 500 - 700 MPa 500 - 700 MPa
Elongation A 40% min 40% min
Hardness 215 HBW max 215 HBW max
Density about 7.9 g/cm3 about 7.9 g/cm3

The mechanical properties in the solution annealed condition are practically identical, so the selection decision is driven by corrosion performance, availability and price rather than by strength. Both grades are non-magnetic in the annealed state and become slightly magnetic after heavy cold working, and both are strengthened only by cold deformation because their austenitic structure cannot be hardened by heat treatment.

Corrosion Resistance, Fabrication and Cost

Aspect 1.4306 1.4307
Nickel content Higher, 10.0 - 13.0% Lower, 8.0 - 10.5%
Corrosion resistance Better in acidic and aggressive media Very good for general purpose service
Weldability Excellent Excellent
Availability Less common Widely available
Relative cost Slightly higher More economical
Typical applications Pharmaceutical, biotech, chemical tanks Kitchenware, storage tanks, general fabrication

Higher nickel improves the stability of the austenitic phase and widens the passivation window, which is why 1.4306 tolerates more aggressive acid exposure and holds up better in installations where repeated cleaning or mildly acidic product contact occurs. The same nickel addition also reduces the risk of delta ferrite and of strain induced martensite forming during severe forming, which matters for deep drawn parts and for components that must stay non-magnetic after fabrication.

Both grades weld readily with TIG, MIG or manual metal arc processes. Because carbon is capped at 0.030%, chromium carbide precipitation in the heat affected zone is limited, so intergranular corrosion resistance is preserved without a post-weld solution anneal in most thicknesses. Pickling and passivation after welding restore the oxide layer where heat tint has formed.

Which Grade Should You Choose?

Choose 1.4307 for the great majority of general fabrications, tanks, kitchen equipment, architectural trim and utility piping. It is widely stocked, easier to source in all product forms and lower in cost.

Choose 1.4306 when the service environment is acidic or otherwise aggressive, when the equipment serves pharmaceutical or biotech duty with frequent aggressive cleaning, or when the part must remain reliably austenitic and non-magnetic after deep drawing.

Consider a higher molybdenum grade such as 316L instead of either, if chlorides are present, because nickel alone does not provide pitting resistance.

FAQ

Q: What is the difference between 1.4306 and 1.4307?
1.4306 contains 10.0 - 13.0% nickel against 8.0 - 10.5% in 1.4307, and its chromium range is 18.0 - 20.0% rather than 17.5 - 19.5%. The higher nickel and chromium give 1.4306 better corrosion resistance in aggressive media at a slightly higher price.

Q: Is 1.4306 better than 1.4307?
It is better only where corrosion demands justify the extra alloy. For ordinary indoor, fresh water and food handling duty the two grades perform similarly and 1.4307 is the more economical choice.

Q: Can 1.4306 and 1.4307 be welded in the same way?
Yes. Both have a maximum carbon content of 0.030% and excellent weldability with conventional TIG, MIG and MMA processes, with minimal post-weld intergranular corrosion risk.

Q: Are both grades classed as 304L?
Yes, both are 304L type low-carbon austenitic grades sharing UNS S30403, and they differ in the nickel level rather than in the carbon limit.

Q: Which grade is more widely available?
1.4307 is the standard commercial 304L grade and is stocked in sheet, plate, tube, bar and fittings. 1.4306 is produced to order more often and can have longer lead times.

Q: Can either grade be hardened by heat treatment?
Neither grade responds to heat treatment hardening because both are fully austenitic. Strength is increased only by cold working such as rolling, drawing or bending.