1.4462 duplex stainless steel equivalent
Jul 17, 2025
Leave a message
What is 1.4462 duplex stainless steel equivalent to?
1.4462 duplex stainless steel, also known as X2CrNiMoN22-5-3, is a widely used grade for its high strength and excellent corrosion resistance, especially in chloride-rich environments.
Material Type: Duplex stainless steel (ferritic-austenitic)
Typical Applications: Pressure vessels, desalination plants, offshore platforms, heat exchangers, pipelines.
| Standard | Equivalent Grade |
|---|---|
| UNS (ASTM/ASME) | S31803 / S32205 |
| AISI / SAE | – |
| JIS (Japan) | SUS329J3L |
| GB (China) | 022Cr22Ni5Mo3N |
| GOST | 08Х22Н5М3Л |
S31803 vs S32205 vs 1.4462: Are They the Same?
While UNS S31803 and 1.4462 are often considered equivalent, UNS S32205 has a slightly optimized composition with improved corrosion resistance. Many manufacturers have shifted from S31803 to S32205 to meet stricter service conditions.
Tip for buyers: If sourcing from Europe, you may receive material labeled as 1.4462 but certified to meet S32205 performance.
Chemical Composition of 1.4462
This chemical balance provides PREN (Pitting Resistance Equivalent Number) of ~34–35, making it suitable for chloride-containing environments like seawater or chemical brine.
| Element | Content (%) |
|---|---|
| Chromium (Cr) | 21.0–23.0 |
| Nickel (Ni) | 4.5–6.5 |
| Molybdenum (Mo) | 2.5–3.5 |
| Nitrogen (N) | 0.14–0.20 |
| Manganese (Mn) | ≤ 2.0 |
| Carbon (C) | ≤ 0.03 |
Mechanical Properties of 1.4462 Duplex Stainless Steel
| Property | Typical Value |
|---|---|
| Yield Strength (Rp0.2) | ≥ 450 MPa |
| Tensile Strength (Rm) | 620–880 MPa |
| Elongation | ≥ 25% |
| PREN (Pitting Resistance) | 34–38 (excellent) |
| Service Temperature | -50°C to +250°C |
What is the density of 1.4462 steel?
| Grade : | X2CrNiMoN22-5-3 | ||
| Number: | 1.4462 | ||
| Classification: | Austenitic-ferritic stainless steel | ||
| Density: | 7.8 g/cm ³ | ||
| Standard: |
|
1.4462 Stainless Steel Machinability & Weldability
Moderate machinability-requires slower cutting speeds and rigid tools compared to austenitic grades.
Good weldability with proper filler metals (e.g., ER2209 or E2209), avoiding excessive heat input to prevent phase imbalance.
Post-weld pickling and passivation recommended for optimal corrosion resistance.
When selecting 1.4462 or its equivalent, consider the operating environment, required certifications, and corrosion resistance levels. Whether you're sourcing from the EU, the US, or Asia, understanding equivalencies ensures quality and compliance.
At GNEE, we supply certified 1.4462 duplex stainless steel pipes, tubes, and sheets with full EN 10204 3.1/3.2 MTC, supporting global equivalents such as S32205. We help clients identify the right grade per project specs and local standards.
1.4462 Duplex Stainless Steel in stock
| Product Form | Size Range (Typical) | Standards |
|---|---|---|
| Seamless Pipe | OD 6 – 610 mm, WT 1 – 50 mm | ASTM A790, EN 10216-5, DIN 17456 |
| Welded Pipe | OD 15 – 1219 mm, WT 1 – 40 mm | ASTM A928, EN 10217-7 |
| Seamless Tube | OD 6 – 114 mm, WT 0.5 – 6 mm | ASTM A789, EN 10216-5 |
| Welded Tube | OD 12 – 254 mm, WT 0.5 – 5 mm | ASTM A249, EN 10217-7 |
| Plate / Sheet | Thickness 1.0 – 50 mm | ASTM A240, EN 10088-2 |
| Coil / Strip | Thickness 0.3 – 6.0 mm, Width up to 1500 mm | ASTM A240, EN 10088-2 |
| Round Bar / Rod | Dia. 6 – 300 mm | ASTM A479, EN 10088-3 |
Surface Finish: 2B, No.1, pickled, polished, or brushed available on request.
Delivery Condition: Solution annealed, pickled, and passivated.
Certifications: EN 10204 3.1 / 3.2, PED/AD 2000, NORSOK (if applicable).


Send Inquiry