304 (1.4301) vs. 904L (1.4539): Industrial Grade vs. Super Austenitic Stainless Steel
Dec 18, 2025
Leave a message



304 (1.4301) - The Workhorse
Type: Standard Austenitic.
Composition: ~18% Chromium, ~8% Nickel (18/8).
Pros: Excellent formability (deep drawing), widely used, cost-effective, good general corrosion resistance (food grade, freshwater).
Cons: Vulnerable to chloride pitting and aggressive chemicals; can suffer intergranular corrosion if welded improperly (hence 304L for low carbon).
Uses: Kitchen sinks, cookware, cutlery, general industrial parts, food processing.
904L (1.4539) - The Specialist
Type: Super Austenitic (High Molybdenum).
Composition: Higher Cr, Ni, plus Molybdenum (Mo) and Copper (Cu).
Pros: Exceptional resistance to pitting, crevice corrosion, stress corrosion cracking, and strong acids (sulfuric, phosphoric); superior to 304/316 in harsh conditions.
Cons: More expensive, slightly harder, less ductile than 304, so harder to form.
Uses: Chemical processing, marine environments, high-chloride areas, flue gas desulfurization, oil & gas.
Key Takeaway
Choose 304 for everyday, general use where cost and formability matter. Choose 904L for severe corrosive environments, strong acids, and high-chloride conditions where superior corrosion resistance justifies the higher cost.