321 and 347H both belong to the 18/8 austenitic family, but they are specified for different ends of the same problem: keeping a welded component corrosion-resistant and creep-resistant while it runs hot. This article compares the two grades on stabilization chemistry, mechanical properties, high-temperature strength, corrosion resistance and fabrication practice, with reference to ASTM A240 and ASTM A312.
How Titanium and Niobium Stabilization Differ
Stabilized grades add a strong carbide former so that carbon is locked into stable carbides instead of reacting with chromium at grain boundaries during welding or high-temperature service. This prevents chromium depletion and intergranular corrosion in the heat-affected zone. 321 uses titanium at a minimum of 5 times the carbon content (0.70% maximum), while 347H uses niobium plus tantalum at a minimum of 8 times the carbon content (1.00% maximum). Because niobium carbides are more stable than titanium carbides at very high temperature, 347H keeps more of its strengthening at service temperatures above roughly 800 °C.
Chemical Composition Compared
Composition ranges per ASTM A240 (wt%):
| Element | 321 / UNS S32100 | 347H / UNS S34709 |
|---|---|---|
| Carbon | 0.08 max | 0.04-0.10 |
| Manganese, max | 2.00 | 2.00 |
| Phosphorus, max | 0.045 | 0.045 |
| Sulfur, max | 0.030 | 0.030 |
| Silicon, max | 0.75 | 0.75 |
| Chromium | 17.00-19.00 | 17.00-19.00 |
| Nickel | 9.00-12.00 | 9.00-13.00 |
| Titanium | 5 x C min, 0.70 max | - |
| Niobium + tantalum | - | 8 x C min, 1.00 max |
Mechanical Properties and High-Temperature Strength
At room temperature both grades meet the same annealed minimums per ASTM A240: tensile strength 515 MPa, yield strength 205 MPa and elongation 40%. The practical difference appears at high temperature. The higher carbon of 347H (0.04-0.10%) combined with niobium carbides provides stronger precipitation strengthening, so 347H retains load-carrying capacity to about 816 °C and shows better creep and rupture strength in long-term service. 321 performs well up to about 760-816 °C and is generally more forgiving under thermal cycling, where its finer, more stable microstructure and better ductility reduce the risk of thermal-fatigue damage.
Corrosion Resistance in Welded Service
Both grades offer excellent resistance to intergranular corrosion after welding, precisely because the stabilizing elements keep carbon out of chromium-carbide form. In mild environments 321 has a slight edge in general corrosion resistance; in high-temperature oxidizing or aggressive service, 347H holds its resistance better over long exposure. Neither grade should be substituted for molybdenum-bearing grades where chloride pitting or crevice corrosion governs the design.
Fabrication and Welding Considerations
321 is more ductile and easier to form into complex shapes, which is why it dominates heat-exchanger tubing and expansion components. 347H requires tighter control of welding heat input and interpass temperature to preserve its high-temperature strength, but it remains workable for most industrial fabrication. Matching filler metals are used: 321-type filler for 321, and 347-type filler for 347H so that the weld metal carries the same niobium stabilization. Post-weld heat treatment is generally not required for either grade.
Application Selection Guide
321 is specified for aircraft exhaust systems, heat exchangers with cyclic heat, expansion bellows and furnace parts where thermal cycling dominates. 347H is specified for power-plant boiler superheater and reheater tubing, high-pressure steam piping, pressure vessels and high-temperature fasteners, typically supplied to ASTM A312 TP347H for pipe and A213 TP347H for boiler tubes. As a rule of thumb, choose 347H where creep strength governs and 321 where formability and thermal cycling dominate.
Frequently Asked Questions
What is the difference between 321 and 347H stabilization?
321 is stabilized with titanium (5 x carbon minimum, 0.70% maximum); 347H is stabilized with niobium plus tantalum (8 x carbon minimum, 1.00% maximum) and carries more carbon (0.04-0.10%) for extra high-temperature strength.
Which grade has better creep strength above 800 °C?
347H. Niobium carbides provide stronger precipitation strengthening than titanium carbides at high temperature, which is why 347H is preferred for pressure parts operating near 816 °C.
Can 321 be substituted for 347H?
For service below about 800 °C where creep is not the governing criterion, 321 can often be substituted. For pressure parts operating above 800 °C, 347H is the safer choice because of its superior creep strength.
Do 321 and 347H resist intergranular corrosion after welding?
Yes. Both are stabilized to prevent chromium-carbide precipitation in the heat-affected zone, so they keep their corrosion resistance in as-welded condition without post-weld heat treatment.
What filler metal should be used for welding?
Use a 321-type filler for 321 and a 347-type filler for 347H so the weld metal carries matching stabilization. Filler selection should also match the governing code (ASME Section IX or equivalent) for the application.
What is the maximum service temperature of these grades?
321 is commonly rated for continuous service to about 816 °C; 347H is rated to about 816 °C with better long-term creep performance in that range. Above these temperatures, oxidation and creep usually force a move to higher-alloy heat-resistant grades.