General Properties

Alloy 347 (UNS S34700) is columbium stabilized austenitic stainless steel plate with good general corrosion resistance and somewhat better resistance in strong oxidizing conditions than 321 (UNS S32100). It has excellent resistance to intergranular corrosion after exposure to temperatures in the chromium carbide precipitation range of 800 – 1500°F (427 – 816°C). The alloy has good oxidation resistance and creep strength to 1500°F (816°C). It also possesses good low temperature toughness.

 

Chemical Analysis

Weight % (all values are maximum unless a range is otherwise indicated)

Element 347 347H
Chromium 17.00 min.-19.00 max. 17.00 min.-19.00 max.
Nickel 9.00 min.-13.00 max. 9.00 min.-13.00 max.
Carbon 0.08 0.04 min.-0.10 max.
Manganese 2.00 2.00
Phosphorus 0.045 0.045
Sulfur 0.03 0.03
Silicon 0.75 0.75
Columbium & Tantalum 10 x (C + N) min.-1.00 max. 8 x (C + N) min.-1.00 max.
Iron Balance Balance

 

 