ASTM A312 UNS S31254 Seamless Pipe: 6% Molybdenum Super-Austenitic Grade

Sep 23, 2025

Leave a message

What Is UNS S31254 Stainless Steel?

UNS S31254 is a fully austenitic, 6% molybdenum super-austenitic stainless steel. It is sometimes described in trade literature as a 6% Mo grade or as a 20Cr-18Ni-6Mo alloy. The steel is solution strengthened and stabilized by nitrogen, and the molybdenum plus nitrogen combination gives it a pitting resistance equivalent number (PREN = Cr + 3.3 Mo + 16 N) of approximately 43, which is roughly double that of 316L. It is important to note that UNS S31254 is not a duplex steel; the microstructure is single-phase austenite, and the grade is non-magnetic in the annealed condition.

The designation is covered by ASTM A312 for seamless and welded pipe, ASTM A269 and A213 for tube, ASTM A240 for plate, and ASTM A182 for forged fittings, with corresponding ASME specifications for pressure service.

Standards and Equivalent Grades

Standard System Designation
UNS (USA) S31254
EN (Europe) 1.4547 / X1CrNiMoCuN20-18-7
AFNOR (France) Z1 CNDU 20.18.06 Az
SIS (Sweden) 2378
Pipe specification ASTM A312 / ASME SA312
Tube specification ASTM A269, A213

Chemical Composition (ASTM A312)

The specified composition of UNS S31254 in ASTM A312 is listed below. The steel is deliberately alloyed with both molybdenum and nitrogen to improve localized corrosion resistance.

Element C Mn P S Si Cr Ni Mo N Cu
Content, % 0.020 max 1.00 max 0.030 max 0.010 max 0.80 max 19.5-20.5 17.5-18.5 6.0-6.5 0.18-0.25 0.50-1.00

Mechanical Properties (ASTM A312)

Seamless and welded pipe of UNS S31254 in the solution-annealed condition meets the following minimum requirements.

Property Requirement
Tensile strength Rm 650 MPa min
0.2% proof stress Rp0.2 300 MPa min
Elongation in 50 mm 35% min

The yield strength of about 300 MPa is noticeably higher than the 205 MPa typical of 304/316 grades, which is one reason the alloy is favored where both strength and corrosion resistance are required.

Heat Treatment

UNS S31254 is supplied in the solution-annealed condition. The recommended annealing temperature is 1150-1200 degrees Celsius, followed by rapid cooling in water or air. Cooling must be fast enough to avoid precipitation of secondary phases, which would reduce corrosion resistance.

Corrosion Resistance and Key Characteristics

Outstanding resistance to pitting and crevice corrosion in chloride media, with a PREN of about 43.

Excellent resistance to chloride stress corrosion cracking, which makes the grade suitable for seawater service where 304 and 316 can fail.

Good resistance to oxidizing acids, and to sulfuric and phosphoric acid environments in many concentrations and temperatures.

Higher strength than 300-series austenitic stainless steels, allowing thinner sections and lighter structures.

Good weldability using matching or over-alloyed filler metals and standard austenitic welding practice.

Typical Applications

Seawater cooling systems, heat exchangers and condensers in power and desalination plants.

Chemical and petrochemical process piping and vessels handling chloride-laden media.

Pulp and paper bleaching equipment.

Flue gas desulfurization (FGD) systems in power generation.

Offshore oil and gas topside equipment and firewater systems.

Food processing equipment where chloride-based cleaning agents are used.

Frequently Asked Questions

Q1. Is UNS S31254 a duplex stainless steel?

No. UNS S31254 has a fully austenitic microstructure. It is a 6% molybdenum super-austenitic grade. Duplex steels such as UNS S32205 have a mixed ferrite-austenite structure and lower nickel content.

Q2. How does S31254 compare with 316L?

S31254 contains about 6% molybdenum versus 2-3% in 316L, plus 0.18-0.25% nitrogen. Its PREN of about 43 is roughly twice that of 316L (about 24), giving far better pitting and crevice corrosion resistance in chloride environments. Its yield strength is also higher (300 MPa versus 170-205 MPa).

Q3. What is PREN and why is it important?

PREN, the pitting resistance equivalent number, is calculated as Cr + 3.3 Mo + 16 N. It is a ranking index for resistance to pitting corrosion in chloride media. Higher values indicate better resistance. S31254 reaches about 43, suitable for seawater and other aggressive chloride service.

Q4. Can S31254 be welded?

Yes. It welds well with GTAW, GMAW, SMAW and SAW using matching filler metals such as EN ISO 18274 Ni-based or over-alloyed 6% Mo consumables. Low heat input and controlled interpass temperatures are recommended, and the steel is usually used in the solution-annealed condition.

Q5. What service temperatures are typical for S31254?

The grade is normally specified for service from about -50 to 300 degrees Celsius in pressure equipment. At higher temperatures the strength decreases, and for continuous elevated-temperature service heat-resistant grades are preferred.

Q6. Why is S31254 called a 6% molybdenum grade?

Because its molybdenum content of 6.0-6.5% is roughly three times that of 316L (2.0-3.0%). Molybdenum is the key element that resists pitting and crevice corrosion in chloride environments, and it works together with nitrogen to strengthen the austenitic matrix.