410 vs 420 Stainless Steel: Low-Carbon vs Medium-Carbon Martensitic Grades Compared
Dec 26, 2025
Leave a message
410 and 420 belong to the martensitic stainless steel family, which is hardenable by heat treatment and magnetic at all temperatures. Unlike austenitic grades, they reach their working strength and hardness through a quench-and-temper cycle: austenitizing dissolves carbides, quenching forms hard martensite, and tempering restores a controlled balance of hardness and toughness. Within the family, 410 represents the low-carbon, weldable end where toughness and fabrication matter, while 420 represents the medium-carbon, hardenable end where wear resistance and cutting performance are the priority.
Chemical Composition
The carbon content is the decisive difference between the two grades; chromium ranges are similar.
| Element, % | 410 (SUS410) | 420 (SUS420J1) |
|---|---|---|
| Carbon (C) | 0.15 max | 0.16-0.25 |
| Silicon (Si) | 1.00 max | 1.00 max |
| Manganese (Mn) | 1.00 max | 1.00 max |
| Phosphorus (P) | 0.040 max | 0.040 max |
| Sulfur (S) | 0.030 max | 0.030 max |
| Chromium (Cr) | 11.50-13.50 | 12.00-14.00 |
| Nickel (Ni) | 0.60 max | 0.60 max |
Equivalent designations: 410 = UNS S41000, EN 1.4006, JIS SUS410; 420 = UNS S42000, EN 1.4021, JIS SUS420J1. The higher-carbon variant 420J2 (0.26-0.40% C) corresponds to EN 1.4028 and is used where maximum hardness is required.
Mechanical Properties and Hardness
Minimum properties in the quenched and tempered condition per JIS G4303, with practical hardness ranges, are shown below.
| Property (quenched and tempered) | 410 (SUS410) | 420 (SUS420J1) |
|---|---|---|
| Tensile strength, MPa | 540 min | 640 min |
| 0.2% proof stress, MPa | 345 min | 440 min |
| Hardness after hardening | about 40-45 HRC | about 50-55 HRC |
| Wear resistance | Moderate | High |
| Impact toughness | Good | Limited; prone to chipping |
The medium carbon of 420 forms a dense dispersion of chromium carbides during hardening, which is the source of its high hardness and edge retention. 410, with less carbon, forms fewer carbides, stops at a lower hardness ceiling, and keeps better ductility.
Heat Treatment
For 410, the standard cycle is austenitizing at about 950-1010°C, oil or air quenching, then tempering at 200-300°C to balance strength and toughness, or at 600-700°C for maximum ductility. Avoid tempering in the range of about 400-550°C, where martensitic 13% chromium steels suffer temper embrittlement and loss of toughness. For 420, austenitize at about 980-1070°C to dissolve the larger volume of carbides, oil quench, then temper at 150-200°C to maximize hardness for cutting tools, or at 250-400°C for a slightly softer, tougher condition. Over-tempering 420 destroys its wear resistance. Both grades are supplied annealed for machining and hardened after final machining, because grinding is difficult at full hardness.
Weldability and Fabrication
410 is the most weldable martensitic grade. It can be joined by GTAW or SMAW with matching 13% chromium filler or austenitic filler, with preheating to 150-250°C and a post-weld temper to relieve residual stress and prevent cold cracking; thin sections can be welded without preheat. 420 behaves differently: the higher carbon promotes hard, crack-sensitive martensite and carbide precipitation in the heat-affected zone, so welding is not recommended for critical load-bearing components without careful preheat, low-hydrogen practice and immediate post-weld tempering. Severe cold working of 420 without intermediate annealing causes work hardening and cracking. Where a welded, hardenable component is required, 410 or a precipitation-hardening grade such as UNS S17400 should be considered.
Corrosion Resistance and Applications
Both grades offer only limited corrosion resistance. 410 tolerates dry indoor conditions, fresh water and mild atmospheres, and is used for pump shafts, valve bodies and stems, steam and gas turbine blades, fasteners, and food machinery parts in dry service. 420, with slightly higher chromium but much higher carbon, has similar or marginally better corrosion resistance in the hardened condition and is used where hardness governs: kitchen knives, scissors, cutting tools, plastic mold cores, valve trim, mechanical seal rings, and textile machine parts. Neither grade suits marine, chloride or acidic service; for those environments select an austenitic grade or a duplex stainless steel, and for hardenable corrosion-resistant parts consider precipitation-hardening grades.
Frequently Asked Questions
Q1: Which grade is harder, 410 or 420? A1: 420. After quenching and tempering it reaches about 50-55 HRC, compared with about 40-45 HRC for 410, because its higher carbon content forms more chromium carbides.
Q2: Can 420 stainless steel be welded? A2: Not reliably. The high carbon causes hard martensite and cracking in the heat-affected zone. For welded hardenable components, use 410 with preheat and post-weld tempering, or a precipitation-hardening grade.
Q3: Do 410 and 420 need heat treatment? A3: To reach full strength and hardness, yes. They are normally supplied annealed for machining, then hardened by austenitizing, oil quenching and tempering before service.
Q4: Are 410 and 420 corrosion resistant? A4: Only to a limited degree. Both tolerate dry indoor conditions but rust in humid, coastal or chemical environments without protective coatings, and neither suits marine or acidic service.
Q5: What is the main compositional difference between 410 and 420? A5: Carbon content. 410 is limited to 0.15% maximum, while 420 contains 0.16-0.25% for SUS420J1. Chromium ranges are similar at 11.5-13.5% and 12-14%.
Q6: What are typical applications of each grade? A6: 410 for welded mechanical parts such as pump shafts, valve bodies, turbine blades and fasteners; 420 for wear and cutting parts such as knife blades, scissors, cutting tools, mold cores and bearing races.
Send Inquiry