Comparison of SUS304 and SUS304L: General-Purpose vs Low-Carbon Austenitic Stainless Steel

Dec 30, 2025

Leave a message

SUS304 and SUS304L are core grades of the 304 series, with the core difference being carbon content (SUS304: C≤0.08%, SUS304L: C≤0.03%). The low carbon content of SUS304L fundamentally avoids intergranular corrosion after welding, making them suitable for different welding process requirements and corrosion environment levels.

info-700-500

Core Parameter Comparison

Parameter

SUS304 Stainless Steel

SUS304L Stainless Steel

Chemical Composition (wt%)

C≤0.08, Si≤1.00, Mn≤2.00, P≤0.045, S≤0.030, Cr=18.00-20.00, Ni=8.00-10.50, Fe=Balance

C≤0.03, Si≤1.00, Mn≤2.00, P≤0.045, S≤0.030, Cr=18.00-20.00, Ni=8.00-12.00, Fe=Balance

Mechanical Properties (Annealed)

Tensile Strength ≥515MPa, Yield Strength ≥205MPa, Elongation ≥40%, Hardness ≤201HB

Tensile Strength ≥485MPa, Yield Strength ≥170MPa, Elongation ≥40%, Hardness ≤201HB

Service Temperature

-196℃ to 870℃ (continuous service)

-196℃ to 870℃ (continuous service)

Equivalent Grades

EN 1.4301, UNS S30400, AISI 304

EN 1.4306, UNS S30403, AISI 304L

info-700-500

Key Performance Differences: 1. Intergranular corrosion resistance: SUS304L's low carbon content prevents the precipitation of Cr₂₃C₆ carbides at grain boundaries during welding, eliminating intergranular corrosion; SUS304 is prone to intergranular corrosion in the weld heat-affected zone if no post-weld annealing is performed. 2. Strength: SUS304 has slightly higher tensile and yield strength than SUS304L due to higher carbon content. 3. Weldability: Both have excellent weldability, but SUS304L does not require post-weld heat treatment for most scenarios, while SUS304 needs post-weld annealing at 850-900℃ for thick plates or harsh corrosion environments. 4. Cost: SUS304L is 5-10% more expensive than SUS304. 5. Formability: Both have excellent cold/hot formability, with no obvious difference.

Applicable Scenario Distinction: SUS304 is suitable for non-welding or post-weld heat-treatable components in general corrosion environments, such as decorative pipes, food machinery (non-welding parts), and indoor storage tanks. SUS304L is suitable for welding-intensive components and medium corrosion environments, such as chemical reaction vessels (welding structure), pharmaceutical equipment, and seawater pipelines (coastal low-salt areas).

info-700-500

Practical Q&A

Q1: Why is SUS304L the preferred material for welding-intensive corrosion-resistant components? A1: Its ultra-low carbon content (≤0.03%) avoids the formation of chromium-depleted zones at grain boundaries during welding, ensuring corrosion resistance of the weld area without post-weld heat treatment, reducing processing costs and improving production efficiency.

Q2: Can SUS304 replace SUS304L in all scenarios? A2: No. In welding-intensive or chloride-containing environments, SUS304's weld area is prone to rust and intergranular corrosion; SUS304 can only replace SUS304L in non-welding scenarios or when post-weld annealing is feasible.

Q3: What is the difference in nickel content between SUS304 and SUS304L? A3: SUS304L has a higher nickel content upper limit (12.00%) than SUS304 (10.50%), which further improves its austenite stability and low-temperature toughness, making it more suitable for ultra-low temperature (-196℃) scenarios.

Q4: What welding materials are suitable for SUS304 and SUS304L? A4: Both can use ER308L welding wire; SUS304L requires stricter control of welding heat input (≤180J/mm) to avoid excessive grain growth, while SUS304 has a wider heat input range.

Q5: How to select between SUS304 and SUS304L? A5: Choose SUS304 if cost is a priority and the component is non-welding or post-weld heat-treatable; choose SUS304L if the component is welding-intensive or used in medium corrosion environments requiring intergranular corrosion resistance.