Common Stainless Steel Grades for Screws
Most stainless steel screws are made from austenitic grades, which combine corrosion resistance, cold formability, and non-magnetic behavior:
201 (UNS S20100): manganese-substituted austenitic grade with roughly 16-18% chromium and 3.5-5.5% nickel plus 5.5-7.5% manganese. Low cost, moderate corrosion resistance; suitable only for dry indoor applications.
304 (UNS S30400): 17.5-19.5% chromium, 8.0-10.5% nickel. The general-purpose grade for indoor and mild outdoor service.
316 (UNS S31600): adds 2.00-3.00% molybdenum. Substantially better resistance to chloride pitting and crevice corrosion; the standard for marine, coastal, and chemical environments.
For bolts, screws, and studs, the governing standard is ISO 3506-1, which uses the letter A for austenitic grades: A1 (free-machining), A2 (304-type), A3 (stabilized 321-type), A4 (316-type), and A5 (stabilized 316Ti-type). The property class follows the letter and hyphen, for example A2-70 or A4-80.
Strength Classes per ISO 3506-1
| Property class | Material group | Min tensile strength (MPa) | Min proof stress 0.2% (MPa) | Typical use |
|---|---|---|---|---|
| A2-50 | 304-type | 500 | 210 | Low-load indoor fasteners |
| A2-70 | 304-type | 700 | 450 | General construction and machinery |
| A4-70 | 316-type | 700 | 450 | Marine and coastal service |
| A4-80 | 316-type | 800 | 600 | High-strength marine and chemical fasteners |
| A3 / A5 | Stabilized (321 / 316Ti-type) | Per class (e.g., 70) | Per class | Elevated-temperature service |
The property class is marked on the head of the screw (for example A2-70 or A4-80) together with the manufacturer symbol, allowing the buyer to verify strength without a test certificate. Austenitic stainless fasteners are not hardened by heat treatment; their strength comes from cold working, and the class defines the minimum properties of the finished product.
Corrosion Considerations and Galvanic Effects
In chloride environments, 316 (A4) screws resist pitting far better than 304 (A2) because molybdenum stabilizes the passive film. However, galvanic corrosion is often the real cause of fastener failure: when stainless steel contacts a more active metal such as carbon steel, aluminum, or zinc in a wet, conductive environment, the more active metal becomes the anode and corrodes rapidly, while the stainless screw is protected. Common examples are stainless screws in aluminum gutters or carbon-steel structures outdoors. Prevention measures include insulating washers and sleeves, compatible material pairs, and keeping the joint dry. In aggressive chloride service, the screw itself should be A4 grade with an appropriate coating or the assembly should be designed so the anode area is large relative to the cathode.
Galling and Seizing: Causes and Prevention
Stainless steel is prone to galling, a form of cold welding in which sliding thread surfaces seize and tear under pressure, especially at high tightening speed. Prevention practices:
Apply a thread lubricant or anti-seize compound rated for stainless.
Control tightening torque and use slow, even speeds; avoid impact driving for final torque.
Use different material pairs where possible, for example a 304 screw in a 316 nut, to break the identical-metal adhesion.
Prefer coated or PTFE-lubricated threads in high-friction assemblies.
Do not rely on heat to free a seized fastener; if a screw has galled, cut it out rather than applying more torque.
Selection Checklist by Environment
Dry indoor air, furniture, electronics: 201 or A2-50/A2-70 304-type.
Humid outdoor, treated timber, mild industrial: A2-70 304-type; verify chloride level.
Coastal air, road-salt exposure, pools, seawater splash: A4-70 or A4-80 316-type.
Chemical plants, food processing with sanitizers: A4-80 316-type; consider coated variants.
Elevated-temperature joints above 300 C: A3 (321-type) or A5 (316Ti-type) stabilized grades to avoid carbide precipitation.
Standards and Marking
ISO 3506-1 covers mechanical properties of corrosion-resistant stainless fasteners; ISO 3506-2 covers nuts, and ISO 3506-3 covers set screws. Dimensional standards for metric screws are ISO 4014/4017 for hex bolts and screws. Where a project code requires traceability, request the material certificate referencing the raw-material standard (e.g., ASTM A276 for bar, EN 10088-3 for rod) and the fastener standard ISO 3506.
FAQ
What do A2-70 and A4-80 mean on a screw head?
The letter and number follow ISO 3506-1: A means austenitic, the digit identifies the material group (2 = 304-type, 4 = 316-type), and the number is the property class, so A4-80 has 800 MPa minimum tensile strength and 600 MPa proof stress.
Which is better for outdoor use: 304 or 316 screws?
In coastal, marine, or de-icing salt environments, 316 (A4) screws, because the molybdenum prevents chloride pitting. For dry and mild inland outdoor use, 304 (A2-70) is normally sufficient and less expensive.
Can stainless screws be used with carbon steel parts?
Not directly in wet service: the carbon steel corrodes rapidly as the anode of a galvanic couple. If the combination is unavoidable, separate the metals with insulating washers and sleeves and keep the joint dry.
Why do stainless screws seize and how can I prevent it?
Seizing, or galling, is cold welding of the thread surfaces under pressure. Prevent it with anti-seize lubricant, controlled torque, slower tightening speed, and different material combinations for screw and nut.
How can I verify the strength of a stainless screw?
Read the head marking, which shows the property class and manufacturer symbol per ISO 3506-1. For critical applications, request the batch test certificate and check the raw-material mill certificate for the grade composition.
Send Inquiry