Key Mechanical Properties at Elevated Temperatures:
Strength Retention: Maintains good tensile and yield strength, crucial for structural integrity under thermal stress.
Creep Strength: Provides excellent short and long-term creep strength for prolonged high-heat exposure.
Oxidation Resistance: Good up to 925°C (1700°F) for continuous service, with scaling starting around 650°C (1200°F).
Temperature Considerations:
Recommended Use: Above 500°C (932°F) for high strength, up to about 800°C (1472°F).
Avoidance Range: Continuous use between 425°C (797°F) and 860°C (1580°F) is generally not recommended due to sensitization, which can reduce corrosion resistance.
Why 304H?
The increased carbon content (0.04-0.1%) provides more strength at high temperatures than 304L (low carbon) or standard 304.