Comparison Of SUS321 And SUS347: Titanium-Stabilized Vs Niobium-Stabilized Austenitic Stainless SteelComparison Of SUS316 And SUS316L: Standard Molybdenum-Containing Vs Low-Carbon Molybdenum-Containing Austenitic Stainless SteelComparison Of SUS304 And SUS316: General-Purpose Vs Molybdenum-Containing Corrosion-Resistant Austenitic Stainless Steel

Chemical Compositions

Element % Present (in product form)
  C, H, P, L TW* / TS*
Carbon (C) ≤0.10 ≤0.15
Silicon (Si) ≤1.50 ≤0.75
Manganese (Mn) ≤2.00 ≤2.00
Phosphorous (P) ≤0.045 ≤0.045
Sulfur (S) ≤0.015 ≤0.030
Chromium (Cr) 24.00 - 26.00 24.00 - 26.00
Nickel (Ni) 19.00 - 22.00 19.00 - 22.00
Nitrogen (N) ≤0.11 -
Iron (Fe) Balance Balance