SUS431 Stainless Steel Chemical Composition
Element | Composition (wt%) | Role/Impact |
|---|---|---|
Carbon (C) | 0.20–0.30% | High carbon content increases hardness and wear resistance after heat treatment. |
Manganese (Mn) | 0.60–1.00% | Improves strength and toughness, especially at lower temperatures. |
Chromium (Cr) | 16.0–18.0% | Provides resistance to corrosion and oxidation, enhancing durability. |
Nickel (Ni) | ≤0.60% | Improves formability and ductility, though lower than in austenitic grades. |
Phosphorus (P) | ≤0.04% | Reduces sulfur contamination and improves machinability. |
SUS431 Stainless Steel Physical Properties
Property | Value | Notes |
|---|---|---|
Density | 7.80 g/cm³ | Slightly denser than other martensitic stainless steels, ensuring durability. |
Melting Point | 1,400–1,530°C | Suitable for both cold and hot working, ideal for high-temperature applications. |
Thermal Conductivity | 26.3 W/m·K | Moderate heat dissipation, suitable for high-heat applications. |
Electrical Resistivity | 7.4×10⁻⁷ Ω·m | Low electrical conductivity, ideal for non-electrical applications. |
SUS431 Stainless Steel Mechanical Properties
Property | Value | Testing Standard/Condition |
|---|---|---|
Tensile Strength | 700 MPa | ASTM A240/A240M standard |
Yield Strength | 500 MPa | Suitable for high-strength applications |
Elongation (50mm gauge) | 15% | Moderate ductility for shaping and forming. |
Brinell Hardness | 450–500 HB | Achieved after heat treatment, offering excellent wear resistance. |
Machinability Rating | 55% (vs. 1212 steel at 100%) | Suitable for machining, though it requires slow speeds to manage hardness. |