What Is 309S Stainless Steel? Composition, Properties and High-Temperature Use
Jun 10, 2025
Leave a message
What Is 309S Stainless Steel?
309S is an austenitic stainless steel with a high chromium content of 22.0-24.0% and a nickel content of 12.0-15.0%, standardized as UNS S30908 under ASTM A240 (plate, sheet and strip). The high chromium content gives it markedly better oxidation resistance at elevated temperature than the 18-8 grades, while the nickel keeps the structure austenitic so that the material stays tough, formable and weldable. The S suffix means low carbon (0.08% maximum), a modification of the original 309 grade that minimizes carbide precipitation and improves weldability. 309S occupies the middle ground of the high-temperature austenitic family: more heat-resistant than 304, but lower in chromium and nickel than 310S (UNS S31008, 24-26% Cr, 19-22% Ni).
Chemical Composition and Mechanical Properties
Chemical composition per ASTM A240 (weight percent)
| Element | 309S (UNS S30908) |
|---|---|
| Carbon (C) | ≤ 0.08 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 0.75 |
| Chromium (Cr) | 22.0 - 24.0 |
| Nickel (Ni) | 12.0 - 15.0 |
Mechanical properties in the annealed condition
| Property | Value |
|---|---|
| Tensile strength, min (MPa) | 515 |
| Yield strength 0.2%, min (MPa) | 205 |
| Elongation, min (%) | 40 |
Elevated-Temperature Behaviour and Applications
The reason to choose 309S is temperature. In continuous oxidizing service, the 22-24% chromium content forms a stable, adherent oxide scale that protects the metal at temperatures where 304 (18% Cr) would scale rapidly and lose section. 309S is therefore used for furnace parts, radiant tubes, burner components, heat-exchanger internals, annealing boxes, kiln furniture and similar duties in petrochemical, power and heat-treatment plant. The low-carbon S version resists sensitization better than standard 309, which matters for welded hot-service construction. For the most severe high-temperature duty - especially cyclic heating and cooling - 310S (UNS S31008) is the usual escalation because of its higher chromium and nickel contents and better scale adhesion.
309 vs 309S
The difference is carbon. Standard 309 (UNS S30900) allows up to 0.20% carbon, which raises hot strength but makes the grade prone to chromium carbide precipitation during welding and in the 400-850 °C service range. 309S limits carbon to 0.08% maximum, which minimizes carbide precipitation and markedly improves weldability and resistance to intergranular corrosion in welded assemblies. For most fabricated hot-service equipment, 309S is preferred; 309 is rarely specified today except where maximum high-temperature strength is required and welding is not involved.
Corrosion Resistance, Magnetism and Limits
At room temperature 309S also offers good general corrosion resistance because of its high chromium content, and it withstands many oxidizing media. Its limits should be understood: like all 18-8 and 25-12 family grades without molybdenum, it has limited resistance to chloride pitting and is not suitable for seawater or strong chloride service - for those duties a molybdenum-bearing grade such as 316L or a duplex grade is the correct choice. In high-temperature service, 309S resists sulfur-containing atmospheres reasonably well in many cases, but carburizing atmospheres should be avoided because chromium carbides can form and degrade the alloy. Is 309S magnetic? No. It is austenitic and essentially non-magnetic in the annealed condition; like other austenitic grades it can develop slight magnetism after cold working because deformation can transform part of the structure. This is normal and does not indicate a quality problem. If a strictly non-magnetic requirement exists, the component should be verified in the annealed condition and by magnetic permeability testing.
FAQ
What is the difference between 309 and 309S?
Carbon content. 309 allows up to 0.20% carbon; 309S limits it to 0.08%. 309S has better weldability and resistance to carbide precipitation, and is the version normally specified today.
What is the maximum service temperature of 309S?
309S is used in continuous oxidizing service at temperatures where 304 cannot be used; in practice it is regularly applied around 1000 °C in oxidizing atmospheres, with the exact limit depending on load, atmosphere and design code. For the most severe cyclic duty, 310S is recommended.
Can 309S be welded?
Yes. It is welded with austenitic filler of the 309 or 310 type, using TIG, MIG or MMA processes. Preheating is not required; the low carbon of 309S keeps the weld heat-affected zone free of significant carbide precipitation.
Is 309S suitable for seawater?
No. Without molybdenum, 309S has limited resistance to chloride pitting and is not suitable for seawater or chloride-laden service. Use 316L or a duplex grade for those environments.
Is 309S the same as 310S?
No. 310S (UNS S31008) has higher chromium (24-26%) and nickel (19-22%), giving better oxidation resistance and scale adhesion at the highest service temperatures. 309S is the lower-alloy, lower-cost member of the pair.
What are the equivalents of 309S?
309S corresponds to UNS S30908 under ASTM A240; the EN 10088 equivalent is 1.4833, and the Japanese designation is SUS309S under JIS G4304/G4305.
Send Inquiry