316Ti Stainless Steel: Titanium-Stabilized High-Temperature Corrosion-Resistant Grade
Dec 18, 2025
Leave a message
316Ti is a titanium-stabilized improved version of 316. By adding 0.10%-0.30% titanium element, titanium combines with carbon preferentially to form TiC, preventing chromium carbide precipitation and completely solving the intergranular corrosion problem of 316 at 400-900℃. It is an ideal material for high-temperature welded structures.

Core Parameters
Chemical Composition (wt%): C≤0.08, Si≤1.00, Mn≤2.00, P≤0.045, S≤0.030, Cr=16.00-18.00, Ni=10.00-14.00, Mo=2.00-3.00, Ti=0.10-0.30, Fe=Balance
Mechanical Properties (Annealed): Tensile Strength ≥515MPa, Yield Strength ≥205MPa, Elongation ≥40%, Brinell Hardness ≤217HB
Service Temperature: 400℃ to 900℃ (continuous service), up to 950℃ for short-term service
Equivalent Grades: SUS316Ti (JIS), EN 1.4571 (EN), UNS S31635 (ASTM)
Performance Advantages: Titanium stabilization enables intergranular corrosion resistance without post-weld heat treatment; high-temperature creep strength is 25% higher than that of 316L; the synergistic effect of molybdenum and titanium provides stronger chloride ion corrosion resistance than 316; oxidation resistance at 900℃ is better than that of 316.
Typical Applications: High-temperature heat exchanger tubes, secondary circuit pipelines of nuclear power plants, chemical cracking furnace tubes, high-temperature heat exchangers of offshore platforms, high-temperature components of semiconductor equipment.

Practical Q&A
Q1: Why should the titanium content of 316Ti be controlled between 0.10% and 0.30%? A1: Below 0.10%, it cannot fully combine with carbon, and there is still a risk of chromium carbide precipitation; above 0.30%, excessive TiN inclusions will form, reducing the toughness and weldability of the steel. The optimal content is 0.20%-0.25%, balancing stabilization effect and mechanical properties.
Q2: Will "titanium burnout" occur when welding 316Ti? A2: Yes. Titanium is prone to oxidation and burnout when the welding temperature exceeds 1200℃. TIG welding should be adopted, with the current controlled at 100-140A, the arc residence time shortened, and pure argon protection used to ensure the titanium content is not less than 0.10%.
Q3: What are the core differences between 316Ti and 316H at high temperatures? A3: 316H improves strength through high carbon and requires prevention of intergranular corrosion after welding; 316Ti achieves corrosion resistance through titanium stabilization, with slightly lower high-temperature strength but more comprehensive corrosion resistance. Choose 316Ti for static high-temperature equipment (such as storage tanks) and 316H for dynamic stress-bearing components (such as transmission shafts).

Q4: Is 316Ti suitable for medical implants? A4: Yes. Its titanium stabilization prevents metal ion leaching, molybdenum improves corrosion resistance to body fluids, and its biocompatibility meets ISO 10993 standards. It can be used for implants such as artificial joints and bone nails, with better performance than 316L.
Q5: How to verify the stabilization effect of 316Ti? A5: Through the Electrochemical Potentiokinetic Reactivation (EPR) test, the reactivation current density is measured, and ≤0.1μA/cm² is considered qualified; or after high-temperature aging (700℃×100 hours), no chromium depletion at grain boundaries is detected.