AISI 316 / EN 1.4401 Stainless Steel Chemical Composition
Nov 27, 2025
Leave a message
What is AISI 316 / EN 1.4401 stainless steel?
AISI 316 / EN 1.4401 is an austenitic stainless steel, designated as AISI 316 under the American standard and EN 1.4401 under the European standard. In the annealed condition, its typical mechanical properties are: tensile strength 480–620 MPa, yield strength ≥170 MPa, elongation >35%, hardness not exceeding 22 HRC (approximately ≤215 HB), density 7.98 g/cm³, and thermal conductivity around 16.3 W/(m·K) at 100 °C. AISI 316 / EN 1.4401 is widely used in chemical equipment, marine engineering, food and pharmaceutical processing, and high-purity gas piping. It can be certified according to standards such as ASTM A240/A479 and EN 10088‑2.
What is the material equivalent to 1.4401?
The 1.4401 material is equivalent to AISI 316 stainless steel. It is also identified by other designations, including UNS S31600 and X5CrNiMo17-12-2.
AISI 316 / EN 1.4401 Stainless Steel Chemical Composition
|
|
C |
Mn |
Si |
P |
S |
Cr |
Mo |
Ni |
N |
|
Min |
|
|
|
|
|
16.0 |
2.0 |
10.0 |
|
|
Max |
0.08 |
2.0 |
0.75 |
0.045 |
0.03 |
18.0 |
3.0 |
14.0 |
0.10 |
1.4401 Mechanical Properties
|
Yield Strength 0.2% (MPa) min |
Tensile strength (MPa) min |
Elongation (% in 50mm) min |
Rockwell B (HR B) max |
Brinell (HB) max |
|
205 |
515 |
40 |
95 |
217 |
1.4401 Physical Properties
|
Density (kg/ m cube) |
Elastic Modulus (GPa) |
Specific heat 0-100°C (J/kg.K) |
Electrical resistivity (nΩ.m) |
|
8000 |
193 |
500 |
740 |
Mean Coefficient of Thermal Expansion (μm/m/°C)
|
0-100°C |
0-315°C |
0-538°C |
|
15.9 |
16.2 |
17.5 |
Thermal Conductivity (W/m.K)
|
at 100°C |
at 500°C |
|
16.3 |
21.5
|
What is 1.4436 equivalent to?
1.4436, 1.4435, and 1.4432 materials are better and more refined equivalents of austenitic 316L steel. The basic difference between grades is the concentration of alloying additives - Nickel, Molybdenum, and Chromium.
What is the difference between 1.4436 and 1.4401?
1.4436 / AISI 316 is an austenitic chromium-nickel-molybdenum stainless steel. 1.4436 is a higher alloyed version of 1.4401 an is specified when the corrosion resistance of 1.4401 is no longer considered to be sufficient.
What is the difference between 1.4404 and 1.4401 material?
The main difference is the carbon content: 1.4401 (AISI 316) has a higher carbon content (up to 0.07%) than 1.4404 (AISI 316L) (up to 0.03%). This lower carbon in 1.4404 makes it better for welding, improving its resistance to intergranular corrosion, and it has superior corrosion resistance and flexibility.
What is the difference between hastelloy and ss316?
Hastelloy has higher nickel and molybdenum contents, making it more resistant in extreme corrosive environments. Stainless steel 316 is the choice for moderately corrosive environments due to its lower cost and wider availability.
GNEE Stainless Steel is an independent stocker and processor of 316/316L stainless steel. With a large inventory and excellent processing capabilities, we can meet the needs of most projects, whether stock products or custom orders. We offer: stock sizes of sheet and slab, stock lengths of round bar, fixed-length sheet and slab, fixed-length round bar, cold forming of sheet and slab and round bar, and any other necessary processing services. For any inquiries, please email sales@gneestainless.com

Send Inquiry