What is X2CrNiMo17-12-2 material?

X2CrNiMo17-12-2 is an austenitic stainless steel, also known as 1.4404 or AISI 316L. This material is a corrosion-resistant alloy containing a high proportion of chromium (Cr), nickel (Ni), and molybdenum (Mo). Due to its durability and resistance to a wide range of corrosive environments, it is commonly used in the chemical, food, and medical industries, as well as in mechanical engineering and equipment engineering.

Other grades: This material also has other grades, such as Z2CND17-12 or S31603.

X2CrNiMo17-12-2 Material

What is ASTM standard for 316L stainless steel?
The primary ASTM standard for 316L stainless steel is ASTM A240, which covers the material in plate, sheet, and strip form. Other relevant standards include ASTM A666 for sheet and strip and ASTM A276 for bars and rods. The ASME standard that corresponds to ASTM A240 is ASME SA240.

 

DIN EN 1.4404 Chemical Composition %

Standard

Steel name (Steel number)

C ≤

Si ≤

Mn ≤

P ≤

S ≤

Cr

Ni

Mo

N ≤

EN 10088-1

X2CrNiMo17-12-2 (1.4404)

0.03

1.00

2.00

0.045

0.030

16.5-18.5

10.0-13.0

2.00-2.50

0.10

 

DIN 1.4404 Physical Properties

Density (g/cm3)

8.0

Thermal conductivity at 20 °C (W/m·K)

15

Specific heat capacity at °C (J/(Kg·K))

500

Electrical resistivity at 20 °C (μΩ·m)

0.75

Magnetic

No

 

Mechanical Properties

Annealed condition for steel sheet, steel plate and steel strip.

Standard

Steel Grade (Steel Number)

Product Condition

Thickness (mm), ≤

0,2 % yield strength (Mpa), (Transverse)

1 % yield strength (Mpa), (Transverse)

Tensile strength (MPa)

Elongation (%), < 3mm thick

Elongation %, ≥ 4mm thick

Impact energy (J) KV2
> 10mm thick (Longitudinal)

Impact energy (J) KV2
> 10mm thick (Transverse)

EN 10088-2

X2CrNiMo17-12-2 (1.4404)

cold rolled strip

8

≥240

≥270

530-680

≥40

≥40

–

–

hot rolled strip

13,5

≥220

≥260

530-680

≥40

≥40

100

60

hot rolled plate

75

≥220

≥260

520-670

≥45

≥45

100

60

 

DIN EN 1.4404 Welding

Compared to stainless steel 1.4401, it can be easily welded using a variety of conventional welding methods due to its extremely low carbon content and does not require annealing after welding.

 

Heat Treatment

Hot forming: 1150 – 850 ℃ (cooling: air)

Solution annealing: 1000 – 1100 ℃ (cooling: water, air)

 

Stainless Steel 1.4404 Hardening

Material 1.4404 can not be hardened by heat treatment but can be hardened by cold working.

 

Applications

1.4404 material is normally firstly processed into many intermediate products such as square steel, round steel, sheet steel, steel strip, steel rods and other forms of steel bars, etc.,

and then processed into finished products such as pipe fittings, angle steel, stainless steel wire mesh, decorative fabrics, filter element, filter cartridges, flanges, valves, elbows, watch straps, etc.

are widely used in aerospace, petrochemical, architectural decoration, and daily necessities industries.

 

If you have any project needs for 316L 1.4404 stainless steel bars, please feel free to place an order. GNEE has a large inventory of popular products for you to choose from. They can be processed into various practical product forms, including plates, coils, pipes, bars, and wires. For detailed chemical composition and free samples, please contact our factory immediately. We offer competitive prices and excellent service.

316L 1.4404 stainless steel

 

Send Inquiry