Composition of grade 431 stainless steel

Table 1. Composition ranges of grade 431 stainless steels

Grade C Mn Si P S Cr Ni
431

min.

max.

-

0.20

-

1

-

1

-

0.04

-

0.03

15

17

1.25

2.50

 

Mechanical Properties of grade 431 stainless steel

Table 2. Mechanical properties of grade 431 stainless steels

Tempering Temperature (°C) Tensile Strength (MPa) Yield Strength 0.2% Proof (MPa) Elongation (% in 50mm) Hardness Brinell (HB) Impact Charpy V (J)
Annealed * 862 655 20 285 max -
204 1345 1055 20 388 50
316 1295 1035 19 375 53
427 1350 1080 19 388 #
538 1140 965 19 321 #
593 1015 770 20 293 64

 

Testing and Documentation: Factory test certificate, EN 10204 3.1, chemical report, mechanical report, destructive testing report, non-destructive testing report, PMI test report, visual inspection report, third-party inspection report, NABL certified laboratory report.
Packaging: Wooden crate packaging, bubble wrap packaging, steel strapping, or packaging according to customer requirements.