What are the core properties of 1.4005 stainless steel?

Apr 02, 2026

Leave a message

1.4005 stainless steel, commonly known as 416 or UNS S41600, is a free-machining martensitic stainless steel specifically designed for high-speed machining applications. With its sulfur addition to improve machinability, it offers the best machinability of all stainless steel grades while maintaining good mechanical properties and moderate corrosion resistance. It is the material of choice for precision components requiring complex machining operations, such as screws, bolts, gears, shafts, and valve components, where production efficiency is critical.

 

Equivalent Grade for 1.4005 stainless steel

Standard Equivalent Grade
EN (Europe) 1.4005
ASTM/AISI (USA) 416, UNS S41600
JIS (Japan) SUS416
KS (Korea) STS416
Common Name 416

 

Chemical composition of 1.4005 stainless steel

Element C Si Mn P S Cr Mo (optional)
Content (%) ≤ 0.15 ≤ 1.0 ≤ 1.25 ≤ 0.06 ≥ 0.15 12.0 - 14.0 ≤ 0.60

 

properties of 1.4005 stainless steel

Condition Yield Strength (Rp0.2) Tensile Strength (Rm) Elongation (A) Hardness (HRC)
Annealed ~ 275 MPa ~ 515 MPa ~ 20% ~ 20 HRC
Hardened & Tempered ≥ 550 MPa ≥ 690 MPa ≥ 15% 30 - 40 HRC

 

Key Characteristics and Applications of 1.4005 / 416

Excellent Machinability: One of the most machinable stainless steels, with machinability approximately 85% of B1112 steel, significantly higher than 304 (45%) and 410 (55%), allowing for high-speed machining, longer tool life, and superior surface finishes.

Good Mechanical Properties: Can be heat treated to achieve good strength and hardness while maintaining adequate toughness for most applications.

Moderate Corrosion Resistance: Provides reasonable resistance to atmospheric conditions, fresh water, mild chemicals, and food acids, but is not suitable for severe corrosive environments like marine or strong acid service.

Magnetic and Heat Treatable: Strongly magnetic and responds well to heat treatment for hardening.

 

Primary Applications:

Fasteners and Fittings: Screws, bolts, nuts, studs, and threaded components produced via high-speed machining.

Precision Components: Gears, shafts, valve stems, pump components, and instrument parts.

Firearms and Defense: Small parts requiring complex machining and good strength.

Medical: Surgical instruments and dental tools requiring precision machining.

General Engineering: Components where machinability is prioritized over maximum corrosion resistance.

Automotive: Fuel injection components and sensor housings.

 

What is the main advantage of using 416 (1.4005) over 410 (1.4006)?

The primary advantage is machinability. 416 is specifically designed for free machining with sulfur additions, allowing for significantly faster cutting speeds, longer tool life, better surface finishes, and lower production costs compared to 410. While 410 has slightly better corrosion resistance and can achieve higher hardness (up to 55 HRC vs. 40 HRC for 416), 416 is the preferred choice for high-volume machined components where production efficiency is critical. For applications requiring maximum hardness and wear resistance, 420 or 440C may be more suitable.

 

How does the sulfur content affect the corrosion resistance of 416?

The high sulfur content (≥0.15%) that improves machinability also forms manganese sulfide inclusions, which can act as initiation sites for pitting corrosion. This reduces the overall corrosion resistance compared to low-sulfur martensitic grades like 410 or 420. Therefore, 416 is not recommended for highly corrosive environments, applications requiring high surface finish integrity, or where the component will be exposed to chlorides, acids, or marine conditions. For such applications, other grades with better corrosion resistance should be considered.

 

What are the heat treatment recommendations for 416?

Typical heat treatment for 416 involves:
Hardening: Austenitize at 980-1030°C, hold for sufficient time, then oil quench
Tempering: Temper immediately after quenching at 540-650°C for optimum toughness, or at 150-370°C for higher hardness
Tempering in the range of 370-540°C should be avoided to prevent tempered martensite embrittlement
Annealing is performed at 830-900°C with slow furnace cooling to soften the material for maximum machinability
 

Looking for a Reliable Supplier of 1.4005 / 416 Stainless Steel?

GNEE Steel supplies free-machining 416 (1.4005) stainless steel in bar, wire, and rod forms, ideal for high-volume machining applications. We provide full material certification (EN 10204 3.1) and processing support including precision cutting and machining services. If you have any requirements, please feel free to contact us.
1.4005 Stainless Steel Pipe

1.4005 Stainless Steel Pipe

1.4005 Stainless Steel Plate1.4005 Stainless Steel Plate

1.4005 Stainless Steel bar

1.4005 Stainless Steel bar

Send Inquiry