What Is 444 Stainless Steel? Composition, Properties and Uses
Jun 11, 2025
Leave a message
444 stainless steel is a ferritic stainless steel with an ultra-low carbon and nitrogen content, about 18 percent chromium and approximately 2 percent molybdenum. Titanium and niobium are added together to stabilize the structure, so the grade resists sensitization even in welded joints. The result is a material whose corrosion resistance approaches or exceeds that of 316 while remaining significantly lower in cost, because it contains little or no nickel. It is magnetic and lower in cost, and it is widely used for water systems, architectural components and automotive service.
What Is 444 Stainless Steel?
444, also written AISI 444 and UNS S44400, is a stabilized ferritic grade built around three ideas. First, chromium at 17.5 to 19.5 percent supplies the passive film. Second, molybdenum at 1.75 to 2.50 percent adds pitting and crevice corrosion resistance, which pushes the pitting resistance equivalent number into the same band as 316. Third, titanium and niobium additions of at least 0.20 percent plus four times the carbon plus nitrogen content lock up the interstitials, preventing the chromium carbide precipitation that would otherwise damage welded joints.
Carbon and nitrogen are both held below about 0.025 percent. That combination of low interstitials plus stabilization gives excellent ductility and toughness for a ferritic grade, and resistance to sensitization even in the weld heat-affected zone.
Composition and Standards
| Element | Content (%) | Role |
|---|---|---|
| C | 0.025 max | Ultra-low to prevent sensitization |
| N | 0.035 max | Ultra-low for toughness and weldability |
| Cr | 17.5 - 19.5 | Passive film |
| Mo | 1.75 - 2.50 | Pitting and crevice corrosion resistance |
| Ti and Nb | 0.20 plus 4 x (C + N) min, 0.80 max | Stabilization against intergranular attack |
| Mn | 1.00 max | Deoxidation |
| Si | 1.00 max | Deoxidation |
| Ni | 1.00 max | Residual only, keeps the grade low cost |
| P | 0.040 max | Residual |
| S | 0.030 max | Residual |
Common product standards and equivalent designations include:
ASTM A240 / A240M - plate, sheet and strip
ASTM A268 - seamless and welded ferritic stainless steel tubing
EN 10088-2 grade 1.4521, formerly X2CrMoTi18-2
JIS G4304 and G4305 grade SUS444
GB/T 4237 grade 019Cr19Mo2NbTi, the current designation that replaced 00Cr18Mo2
Mechanical and Physical Properties
| Property | Typical value |
|---|---|
| Tensile strength | 415 MPa min |
| Yield strength (0.2% offset) | 275 MPa min |
| Elongation in 50 mm | 20% min |
| Hardness | 217 HBW max |
| Structure | Ferritic, magnetic |
| Thermal expansion | Lower than 304, close to carbon steel |
| Thermal conductivity | Higher than austenitic grades |
The physical behaviour is a major practical advantage. A lower coefficient of thermal expansion and higher thermal conductivity than 304 or 316 reduce thermal stress and improve heat transfer, which is why the grade is common in water heating equipment. Ferritic grades also resist chloride stress corrosion cracking far better than austenitic grades, because chloride stress cracking is an austenitic failure mode.
Two limits should be respected. Long exposure to temperatures around 475 degrees C causes the embrittlement typical of molybdenum-bearing ferritic steels, and exposure above roughly 600 degrees C can form sigma phase. Long-term service is therefore normally kept below about 400 degrees C.
316, 304 and 444: How They Compare
| Feature | 444 | 316 | 304 |
|---|---|---|---|
| Structure | Ferritic, magnetic | Austenitic, non-magnetic | Austenitic, non-magnetic |
| Nickel content | 1.0% max | 10 - 14% | 8 - 10.5% |
| Molybdenum | 1.75 - 2.50% | 2 - 3% | None |
| Pitting resistance | Comparable to 316 | Good | Moderate |
| Chloride stress cracking | Resistant | Susceptible | Susceptible |
| Tensile formability | Good | Excellent | Excellent |
| Relative cost | Lower | Higher | Moderate |
The comparison with 316 comes down to two points. The cost of 316 is higher mainly because of its high nickel content. 316 also offers better tensile formability, which makes it more advantageous where high ductility is required, and 316 is non-magnetic while 444 is magnetic. In exchange, 444 gives comparable pitting resistance at lower cost, better resistance to chloride stress corrosion cracking, and better heat transfer behaviour.
444 should also be distinguished from the titanium-stabilized 443 grade, which relies on chromium and titanium without a deliberate molybdenum addition. The molybdenum in 444 is what delivers its pitting and crevice corrosion performance, and the two grades should not be treated as interchangeable.
Typical Applications
Water heating: inner tanks for domestic hot water heaters and solar hot water systems
Heat exchanger tubing for fresh water and mildly corrosive media
Construction engineering: bridge guardrails, structural components, roofing, gutters and architectural panels
Automotive manufacturing: exhaust system components and related engine parts
Food industry: processing equipment and packaging container components
Medical device industry: protective and structural material for precision instruments and equipment
Dishwasher and kitchen appliance components, sinks and process tanks
In these duties the combination of corrosion resistance, lower cost and good processing performance is what justifies the grade. Where deep drawing or severe stretch forming is required, an austenitic grade is still the safer choice.
Frequently Asked Questions
Q: What is 444 stainless steel?
It is a low-carbon, low-nitrogen ferritic stainless steel containing about 18 percent chromium and 2 percent molybdenum, stabilized with titanium and niobium. It offers excellent ductility, toughness and resistance to sensitization, even in welded joints, and is magnetic.
Q: Is 444 stainless steel magnetic?
Yes. Its ferritic crystal structure is ferromagnetic, so 444 is magnetic in all conditions, unlike the austenitic 304 and 316 grades, which are essentially non-magnetic when annealed.
Q: What is the difference between 316 and 444?
316 is austenitic, non-magnetic and rich in nickel, which is the main reason it costs more. 316 also has better tensile formability. 444 is a lower-cost, magnetic ferritic grade with molybdenum that provides comparable pitting resistance and clearly better resistance to chloride stress corrosion cracking.
Q: Is 444 better than 304 or 443 stainless steel?
For corrosion resistance, 444 is generally a step above 304 because of its molybdenum content. The titanium-stabilized 443 grade contains chromium and titanium without molybdenum, so it offers good high-temperature stability but lower pitting resistance than 444. The right choice depends on the corrosion duty rather than on the grade number alone.
Q: What are the components of 444 stainless steel?
444 contains 17.5 to 19.5 percent chromium, 1.75 to 2.50 percent molybdenum, carbon and nitrogen each held near or below 0.025 percent, and titanium plus niobium at a minimum of 0.20 plus four times the carbon plus nitrogen content to stabilize the structure.
Q: Where is 444 stainless steel used?
It is widely used for hot water tanks, solar water heating systems, heat exchanger tubing, bridge guardrails and architectural components, automotive exhaust parts, food processing equipment and precision medical instruments.
Send Inquiry