What material is 1.4021 X20Cr13?
Aug 21, 2025
Leave a message
What is 1.4021 stainless steel?
DIN 1.4021 stainless steel, also known as X20Cr13, is a martensitic stainless steel with a high carbon content (0.16-0.25%) and a high chromium content (12-14%). This composition gives it excellent mechanical properties, including high strength and hardness after tempering, as well as good corrosion resistance. It is often used in applications requiring a combination of strength, hardness, and moderate corrosion resistance.
What is 1.4021 material ASTM equivalent?
| DIN EN X20Cr13 (1.4021) Material Equivalent | |||||||||
| European Union | US | ISO | China | Japan | |||||
| Standard | Steel Name (Material Number) | Standard | Grade (UNS) | Standard | Grade (ISO number ) | Standard | Grade | Standard | Grade |
| EN 10088-2; EN 10088-3; EN 10088-1 |
X20Cr13 (1.4021) | AISI; ASTM A240/A240M; ASTM A276/A276M; ASTM A959 |
AISI 420 (UNS S42000) |
ISO 15510 | X20Cr13 (4021-420-00-I) | GB/T 1220; GB/T 3280 |
2Cr13; 20Cr13 (New designation) | JIS G4303; JIS G4304 |
SUS 420J1 |
What is the composition of X20Cr13?
| Chemical Composition, % | |||||||
| Standard | Steel Grade (Steel Number) | C | Si, ≤ | Mn, ≤ | P, ≤ | S, ≤ | Cr |
| EN 10088-2; EN 10088-3 |
X20Cr13 (1.4021) | 0,16-0,25 | 1,00 | 1,50 | 0,040 | 0,015 | 12,0-14,0 |
EN 1.4021 Stainless Steel Mechanical Properties
| Mechanical Properties | |||||||||||
| Country (Region) | Standard | Steel Grade (Steel Number) | Product Condition | Heat treatment condition | Thickness (mm), ≤ | Hardness, HRB (HBW or HV) | 0,2 % yield strength, Mpa (ksi), ≥ | Tensile strength, Mpa (ksi) | Elongation, %, ≥, (long. + tr.) | Impact energy (ISO-V), KV2 >10mm thick, ≥ J | Rockwell Hardness, HRC (HV) |
| European Union | EN 10088-2 | X20Cr13 (1.4021) | cold rolled strip | +QT | 3 | – | – | – | – | – | 44-50 (440-530) |
| cold rolled strip | +A | 8 | 95 (225) | – | 700 (101), ≤ | 15 | – | – | |||
| Hot rolled strip | +A | 13,5 | |||||||||
| Hot rolled plate | +QT650 | 75 | – | 450 (65) | 650-850 (94-123) | 12 | by agreement | – | |||
| Hot rolled plate | +QT750 | 550 (80) | 750-950 (108-137) | 10 | |||||||
| Notes: +A: Annealed, +QT: Quenched and Tempered. |
|||||||||||
Corrosion Resistance:
1.4021 offers good resistance to various media, including non-chlorine-containing environments like organic acids, soaps, and solvents, as well as steam and freshwater. However, it's not suitable for highly corrosive environments like marine or chloride-rich conditions.
EN 1.4021 Heat Treatment Conditions:
QT700:
Hardening at 950-1050°C (1742-1922°F) and tempering at 650-750°C (1202-1382°F).
QT800:
Hardening at 950-1050°C (1742-1922°F) and tempering at 600-700°C (1112-1292°F).
Is 1.4021 magnetic?
1.4021 stainless steel is a martensitic grade of stainless. It is magnetic and hardenable with rust resistant properties.
What material is 1.4021 QT800?
EN 1.4021 +QT800 steel is EN 1.4021 stainless steel in the quenched and tempered condition. It has the highest strength compared to the other variants of EN 1.4021 stainless steel.
If you have a project need for sus420j1 1.4021 stainless steel bar, we welcome your order. GNEE has a large inventory of popular products for you to choose from. We process these bars into a variety of practical product forms, including sheet, coil, tube, bar, and wire. For detailed chemical composition and free samples, please contact our factory today. We offer competitive pricing and excellent service.Email: sales@gneestainless.com