what is the F44 / 254SMO (UNS S31254)?

254SMO (F44, UNS S31254, 1.4547) is an ultra‑low‑carbon super austenitic stainless steel with high molybdenum plus nitrogen alloy design, reaching a PREN of 42‑45. It excels at resisting chloride‑induced pitting and crevice corrosion, performing well in high‑chloride service such as seawater, brine and flue gas desulfurization. With higher mechanical strength, it is widely used in seawater desalination, offshore platforms and FGD systems. It is not suitable for pure reducing acid environments.

 

what is the 904L(UNS N08904,1.4539)?

904L (UNS N08904, 1.4539) is an ultra‑low‑carbon super austenitic stainless steel featuring higher nickel content and copper addition. Copper greatly improves its resistance to reducing acids such as dilute sulfuric acid and phosphoric acid. Its PREN is only 34‑36, so its chloride corrosion resistance is inferior to 254SMO, and long‑term immersion in seawater is not recommended. It is mainly applied for acidic processes including wet‑process phosphoric acid, dilute sulfuric acid chemical production and pharmaceutical equipment.

904L seamless steel pipe

904L seamless steel pipe

254SMO Hexagonal Bar

254SMO Hexagonal Bar

254SMO F44 Forged Flange

254SMO F44 Forged Flange

If you need specific help, please share:

Are you looking for pipes, tubes, or fittings?

What is your required size and schedule?

What fluid or chemical environment will it be exposed to?

Contact now

Grade Overview & Standard Designation of F44 / 254SMO (UNS S31254) and 904L (UNS N08904)

The two materials correspond to different international standard numbers, covering UNS, European and Chinese national standards, which are widely recognized in global industrial procurement.

Item

254SMO (F44)

904L

UNS Number

S31254

N08904

W.Nr / EN Standard

1.4547

1.4539

GB Standard

022Cr20Ni18Mo6CuN

015Cr21Ni26Mo5Cu2

Forging Grade

ASTM A182 F44

-

 

Chemical Composition (wt%) of F44 / 254SMO and 904L

The core performance difference comes from alloy ratios. 254SMO adopts high Molybdenum and Nitrogen reinforcement for chloride resistance, while 904L uses higher Nickel and Copper to optimize acid resistance.

Element

254SMO (S31254)

904L (N08904)

C (max)

0.020

0.020

Cr

19.5–20.5

19.0–23.0

Ni

17.5–18.5

23.0–28.0

Mo

6.0–6.5

4.0–5.0

Cu

0.5–1.0

1.0–2.0

N

0.18–0.22

≤0.10

PREN Value

42–45

34–36

PREN (Pitting Resistance Equivalent Number): Higher values mean stronger resistance to pitting and crevice corrosion in chloride environments.

 

Mechanical Properties of F44 / 254SMO and 904L (Solution Annealed, Room Temperature)

Benefiting from nitrogen solid solution strengthening, 254SMO possesses higher mechanical strength than 904L, making it more suitable for high-pressure structural parts.

Performance Parameter

254SMO (F44)

904L

Tensile Strength (MPa, min)

650

490

0.2% Yield Strength (MPa, min)

300

220

Elongation A5 (%, min)

35

35

Max Hardness (HB)

220

250

 

Corrosion Resistance Comparison of F44 / 254SMO and 904L

1.Chloride & Seawater Environment

254SMO shows absolute advantages. Its high PREN value ensures excellent resistance to pitting and crevice corrosion. It can withstand long-term service in high-temperature seawater, brine, and flue gas desulfurization environments.

904L has limited chloride resistance. With a lower PREN value, it is only suitable for low-concentration and low-temperature chloride conditions. Long-term seawater immersion will cause severe pitting corrosion.

 

2.Reducing Acid Environment

904L performs better. The high copper content stabilizes the passive film in dilute sulfuric acid, phosphoric acid and acetic acid, providing outstanding resistance to reducing acid corrosion.

254SMO is not ideal for pure reducing acid working conditions, and its acid resistance is obviously inferior to 904L.

 
3.Intergranular & Stress Corrosion

Both materials adopt ultra-low carbon design, effectively avoiding intergranular corrosion after solution annealing. 904L with higher nickel content has excellent stress corrosion resistance, while 254SMO is more reliable in high-chloride stress corrosion scenarios.

 

Typical Industrial Applications

Applications of 254SMO (F44 / S31254)

Seawater desalination equipment, offshore platform piping and cooling systems

FGD flue gas desulfurization towers and high-chloride wastewater treatment facilities

Pulp and paper bleaching equipment, high-chloride chemical heat exchangers

High-pressure corrosion-resistant pipelines and flange forgings

 

Applications of 904L (N08904)

Wet-process phosphoric acid and dilute sulfuric acid chemical reactors and heat exchangers

Pharmaceutical, fertilizer and pickling industrial equipment

Medium-corrosion industrial systems with low chloride content

Offshore platform piping

Offshore platform piping

Chemical pipelines

Chemical pipelines

Food and Pharmaceutical Pipeline

Food and Pharmaceutical Pipeline

If you are specifying this material for a project, let me know:

What is the specific chemical environment or operating temperature?

Do you need data on specific product forms (e.g., plate, seamless pipe, bar, or fittings)?

Contact now

Welding & Processing Notes

Both are fully austenitic stainless steels with high work hardening rate, requiring low-speed cutting and sufficient cooling during machining.

254SMO: Matched with nickel-based welding wires such as ERNiCrMo-3

904L: Matched with professional ER385 welding consumables

Strictly control welding heat input and interlayer temperature to maintain original corrosion resistance

 

Selection Quick Reference

For chloride‑rich environments, prefer 254SMO (F44); for dilute sulfuric acid / phosphoric acid service, prefer 904L

Working Condition Recommended Material Remarks
Seawater immersion, brine, high‑temperature high‑chloride media 254SMO (F44) PREN>40, good resistance to crevice corrosion
Dilute sulfuric acid, 85% phosphoric acid, reducing acid service 904L Copper alloying delivers excellent acid resistance
Acid mixed with high content of chloride ions 254SMO (F44) Balances acid and chloride corrosion resistance
Medium corrosion with limited budget and low chloride level 904L Relatively lower cost and wide availability

 

FAQ

1.Can 904L replace 254SMO for seawater service?

Not recommended. 904L has a low PREN value and poor seawater corrosion resistance. Long-term seawater immersion will cause crevice corrosion and pitting. 254SMO is the preferred material for seawater working conditions.

 

2.Which material is better for sulfuric acid resistance?

904L is superior in pure dilute sulfuric acid and phosphoric acid environments. If the acid medium contains a large amount of chloride ions, 254SMO is a more reliable choice.

 

3.Which material has higher mechanical strength?

254SMO has a yield strength of no less than 300MPa, much higher than 904L (220MPa). It can reduce wall thickness and save costs for pressure-bearing equipment.

 

4.What is the core selection principle of the two materials?

Choose 254SMO for high chloride, seawater and desulfurization working conditions; Choose 904L for dilute sulfuric acid, phosphoric acid and general acidic chemical working conditions.

 

5. Are both materials resistant to intergranular corrosion?

Yes. Both are ultra-low-carbon super austenitic stainless steels. After standard solution annealing treatment, they have excellent intergranular corrosion resistance.

 

Send Inquiry